At present, the glass fiber reinforced bars on the market already have good cuttability. Due to the light weight and toughness of the material itself, some traditional cutting tools, such as electric saws, steel hammers, and pliers, can be used for processing. In addition, there are also some special fiberglass rebar cutting tools, such as abrasive cutting machines, electric saw cutting machines, etc., which can be cut more conveniently and quickly.
It should be noted that when cutting glass fiber reinforced bars, attention should be paid to safety, to avoid dust and other harmful substances, and the accuracy and quality of cutting must be guaranteed, otherwise the use effect and safety may be affected.
Products Description:
FRP (Fiber Reinforced Polymer) rebars are a type of reinforcement bar used in construction that is made of composite materials consisting of high-strength fibers embedded in a polymer matrix. FRP rebars offer several advantages over traditional steel reinforcement, including higher strength-to-weight ratio, corrosion resistance, and non-magnetic properties.
Feature:
High Tensile Strength: The load is approximately double that of a steel bar with the same diameter
Low Weight: The labor intensity is greatly reduced, and the transportation cost is reduced at the same time;
Anti static: It has noelectrical conductivity, and no sparks will be produced when being cut. It is particularly suitable for high gas zones;
Non-flammable: It is non-flammable and has high thermal insulation;
Cuttability: It avoids damages to cutter heads,and does not delay excavation
Save cost: Use this material as reinforcing bars for road and bridge, could reduce Secondary repair cost.
| Product Specification | |||
| Specification | yft100-25-12 | Name | Hollow Rockbolt |
![]() |
|||
| Item | Unit | Permissible Deviation | Standard Parameter |
| Outer Diameter (Da) | mm | ±0.5 | 25 |
| Measure Bottom Diameter (Db) | mm | ±0.5 | 22.6 |
| Diameter of the hole | mm | ±0.5 | 12 |
| Effective Diameter (Dd) | mm | ±0.5 | 22 |
| Screw Pitch (P) | mm | ±0.2 | 10 |
| Rod Length (L) | mm | ±10 | |
| Active Section | mm² | — | 267 |
| Weight | g/m | ±25 | 640 |
| Fiberglass Content | % | ±5 | 80 |
| Density | g/cm³ | ±0.1 | 2 |
| Ultimate Load-bearing | kN | ≥ | 220 |
| Ultimate Tensile Strength | MPa | ≥ | 820 |
| Shear Strength | MPa | ≥ | 150 |
| Elastic Modulus | GPa | ≥ | 40 |
| Ultimate Strain | % | ≥ | 1.2 |
| torsional strength | N·m | ≥ | 100 |
| Nut bearing capacity | kN | ≥ | 100 |